该厂于1973年3月开始处理深泽矿,1979年10月混合处理深泽和饵钓矿矿石。选矿厂能力从2万吨/月增至3万吨/月。选矿厂使用棒磨机一台,球磨两台构成与水力旋流器成闭路的三段磨矿流程。矿石磨碎至—200目占85%,浮选为铜铅—锌硫化铁混合优先浮选。选矿厂近年由于引进了在流分析装置,实现了铜铅半混合浮选、锌浮选药剂自
The plant started processing the deep-seated ore in March 1973 and mixed with the deep-seated and baited-ore ore in October 1979. Concentrator capacity from 20,000 tons / month to 30,000 tons / month. Concentrator using a rod mill, ball mill and hydrocyclone form a closed three-stage grinding process. Ore grinding to -200 mesh accounted for 85%, flotation of copper and lead - zinc ferric sulfide preferential flotation. Concentrator in recent years due to the introduction of the flow analysis device to achieve a copper-lead semi-mixed flotation, zinc flotation agent since