论文部分内容阅读
通过控制化学成分、优化热轧工艺和冷轧工艺,降低了冷轧低碳钢DC01的屈服强度,使冷轧低碳钢DC01的力学性能合格率达到99.58%,为生产出满足市场需求的冷轧低碳钢DC01产品奠定了良好的工艺基础。
By controlling the chemical composition, optimizing the hot rolling process and the cold rolling process, the yield strength of the cold-rolled low-carbon steel DC01 is reduced so that the mechanical performance pass rate of the cold-rolled low-carbon steel DC01 reaches 99.58%. In order to produce the cold Rolling low carbon steel DC01 products laid a good foundation for the process.