由冶金部、机械部协作组织的高速钢攻关组,经过几年的努力,研制了W9Mo3Cr4V(简称9341)高质量通用高速钢。它兼有W18Cr4V、W6MoSCr4V2钢的优点,而避免了两者的不足。9341钢原材料来源丰富,适合国情。从1981年起经在12个大工具厂试用并投放市场,用户反映良好。实践证明,9341钢是一种综合性能较好,特别是工艺性能良好,切削寿命较长,有推广价值的新钢种。 By the Ministry of Metallurgical, Mechanical Department of high-speed steel collaborative organization attack group, after several years of efforts, developed W9Mo3Cr4V (referred to as 9341) high-quality general-purpose high-speed steel. It combines the advantages of W18Cr4V, W6MoSCr4V2 steel, while avoiding the deficiencies of both. 9341 steel source rich, suitable for the national conditions. From 1981 onwards in 12 large tool factory trial and put on the market, the user reflects the good. Practice has proved that 9341 steel is a good overall performance, in particular, good process performance, long cutting life, a promotional value of the new steel.
其他文献
新日本钢铁公司采用一种新的切分轧制法生产圆钢和螺纹钢。新的切分轧制法称为“多条切分轧制法”,钢坯靠轧辊进行切分,而不使用任何特殊的切分装置。切分数量可自由选择,以
图中所示刀具是专为电扇马达轴承座设计的内球面挤压刀。内球面挤压前可直接用成型刀鍯出,但要注意孔口直径不能大,否则达不到挤压效果。一、挤压片和刀体挤压片可直接在车
我厂生产的可锻铸铁阀体在24kgf/cm~2水压试验时发生渗漏,严重影响了产品送检合格率。究其原因,主要有三方面。一是缩松,二是裂纹,三是夹渣。经分析绝大部分是由缩松缺陷引
00593 Fabrication of 0.1μm-Gate InP HEMTs Using i-Line Lithography/K. Sawada,K. Makiyama, T. Takahashi et al (Fujitsu Laboratories Ltd, Japan)//2003 Indium Ph
提起王志文、许晴、巍子,恐怕无人不知,无人不晓。今年这三位影视界的当红明星不约而同来到《DA师》剧组,共同演绎了一回当代军人的崭新形象。 由中央电视台影视部和前线话
一、前言轧制6.5mm盘条所用的轧辊,选用瓦房店轴承厂生产的GCr15钢,经锻造成型及轧后球化退火,机械加工成轧辊后,最终淬火加低温回火处理。 1985年4月生产的14个轧辊,经机械
现在,已经研究成功不少F_4表面处理技术。但各有利弊,适用性不同。本工作选择具有代表性的钠—萘络合物法、醋酸钾热熔法、辉光放电法作对比试验,从而得出了一些具有实际意
大智公司是青浦工业园区的一家民营企业,公司成立6年来,从数百万元起家至今资产近亿元,去年的销售额达3.6亿元,预计今年将超过5亿元。大智集团最早是生产塑料薄膜,工农业用
一、三年多来成效显著三年多来,龙岗区本届政府在市委市政府和区委的正确领导下,以邓小平理论和“三个代表”重要思想为指导,全面贯彻落买科学发展观,求真务买,开拓进取,推动
以哈尔滨市二轻研究所侯振淑工程师和哈尔滨汽车电器厂赵永祚工程师为主的课题组,研制的组合冲模最近通过了省级鉴定。为在国内中小工厂推广应用,现将这项先进组合冲模介绍