论文部分内容阅读
To acquire a well bonded interface between the copper and the diamond particles in diamond-copper matrix composites, an available process to apply a vapor deposited aluminum (Al) coating onto diamond particles was used to solve this interfacial problem. The diamond-copper matrix composites were prepared by spark plasma sintering (SPS) process and the effect of Al-coated diamond particles was demonstrated. The experimental results showed that the densification, interfacial bonding and thermal conductivity of Al-coated composites were evidently improved compared to those of the uncoated composites. A maximum thermal conductivity (TC) of 565 W/(m?K) was obtained in the coated composite containing 50vol%diamond particles sintered at 1 163 K. Additionally, the experimental data of thermal conductivity and coefficient of thermal expansion (CTE) were compared with the predictions from several theoretical models.